Shashwat Stainless Inc is a Top Manufacturer of Duplex Steel & Super Duplex Steel in India. We are an ISO 9001:2008 certified company Incepted in 2007, Shashwat Stainless Inc is promoted by a group of highly experienced technical personnel having rich experience in the Field of manufacturing of Duplex Steel & Super Duplex Steel, Buttweld Fittings, Forged Fittings & Flanges. Shashwat Stainless Inc, today are one of India′s emerging companies involved in the Manufacturing and Supplying of quality Stainless Steel, Alloy Steel, Carbon Steel, Pipes & Tubes Fittings, Forged Fittings and many more

Company profile

Headquarters

Mumbai, India

Type

Manufacturer and Distributor

Certifications

ISO 9001

, ISO 9001

, ISO 14001

, OHSAS 18001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

17-4 PH

Bar, Profile, Angle

17-4 PH, UNS S17400

AISI 304

Pipe

AISI 304

AISI 316

Pipe

AISI 316

ASTM F51

Bar, Angle, Profile

ASTM F51, DIN 1.4462

ASME SA 276, ASTM A276

ASTM F53

Bar

ASTM F53

UNS S31254

Bar

UNS S31254, DIN 1.4547

ASTM A276

UNS S31803

Bar

UNS S31803

ASTM A276

UNS S32205

Bar, Angle, Profile

UNS S32205

ASTM A276

UNS S32750

Bar

UNS S32750

ASTM A276

UNS S32760

Bar, Angle, Profile

UNS S32760, Duplex 2507

ASTM A276