Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN Cu-ETP

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN Cu-ETP

EN Cu-HPC

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN Cu-HPC

EN Cu-OF

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN Cu-OF

EN CuBe1

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuBe1

EN CuBe2

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuBe2

EN CuCr

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuCr

EN CuCr1Zr

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuCr1Zr

EN CuNi14Al3

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuNi14Al3

EN CuNiBe

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuNiBe

EN CuSi0.12

Casting, Forging, Plate, Ring, Extrusion, Bar, Profile

EN CuSi0.12

Showing 1 to 10 of 19 entries

Previous

1
2

Next

Locations

Italy

Italy

Via Bainsizza 37/38

20814 VAREDO,Monza e della Brianza

(+39)0362544133

Italy

Via G. Puccini 21

20028 SAN VITTORE OLONA,Milan

(+39)0331423011