Our business was originally focused on warehousing and distribution of steel from a single facility with no major processing equipment. Today, our enterprise has an enormously wider range, focused on growth, geographic and customer diversity, and the value-added processing of flat-rolled metals and pipe and tube
Headquarters
HIGHLAND HILLS,Ohio, United States
Website
Type
Manufacturer and Distributor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 1006 | Coil, Sheet | AISI 1006 | |
AISI 1008 | Coil, Sheet | AISI 1008 | |
AISI 1010 | Coil, Sheet | AISI 1010 | |
AISI 1012 | Coil, Sheet | AISI 1012 | |
AISI 1015 | Coil, Sheet | AISI 1015 | |
AISI 1018 | Coil, Sheet | AISI 1018 | |
AISI 1019 | Coil, Sheet | AISI 1019 | |
AISI 1020 | Coil, Sheet | AISI 1020 | |
AISI 1021 | Coil, Sheet | AISI 1021 | |
AISI 1022 | Coil, Sheet | AISI 1022 | |