Fowle and Co Group is one of the largest independent sheet steel stockists and processors in the UK.
Headquarters
East Sussex, United Kingdom
Website
Type
Manufacturer, Processor and Distributor
Certifications
ISO 45001
, ISO 9001
Grade | Shape | ||
---|---|---|---|
EN DC01 | Sheet | EN DC01 | EN 10130 |
EN DC02 | Sheet | EN DC02 | EN 10130 |
EN DC03 | Sheet | EN DC03 | EN 10130 |
EN DC04 | Sheet | EN DC04 | EN 10130 |
EN DD11 | Sheet | EN DD11 | EN 10111 |
EN DX51D | Sheet | EN DX51D | EN 10346 |
EN S220GD | Sheet | EN S220GD | EN 10346 |
EN S275 | Sheet | EN S275 | EN 10111 |
EN S280GD | Sheet | EN S280GD | EN 10346 |
EN S355 | Sheet | EN S355 | EN 10111 |