Titanium Solutions GmbH

Claim this profile

About Titanium Solutions GmbH

Starting with simply trading titanium, we now have the option of offering our customers customised titanium and cobalt-chrome products from manufacturing channels monitored in-house from the raw material to the finished part.

Company profile

Headquarters

Bremen, Germany

Type

Manufacturer and Processor

Certifications

ISO 9001

, EN 9100

, ISO 13485

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN CoCrMo

Forging

EN CoCrMo

ISO 22674

EN CoCrWMo

Forging

EN CoCrWMo

ISO 22674

GHOST VT16

Wire, Rod

GHOST VT16

GOST 19807

Ti-6Al-2Sn-4Zr-2Mo

Bar

Ti-6Al-2Sn-4Zr-2Mo

Ti-6Al-2Sn-4Zr-6Mo

Bar

Ti-6Al-2Sn-4Zr-6Mo

AMS 4981

Ti-6Al-4V

Bar, Wire, Rod

Ti-6Al-4V, Titanium Grade 5

AMS 4928, ASTM B348

Ti-6Al-4V (ELI)

Bar, Wire, Rod

Ti-6Al-4V (ELI), Titanium Grade 23

ASTM F136, ISO 5832-3, ISO 4930

Ti-6Al-7Nb

Bar, Wire, Rod

Ti-6Al-7Nb

ASTM F1295, ISO 5832-11

Ti-7Al-4Mo

Bar

Ti-7Al-4Mo

AMS 4970

Titanium Grade 1

Bar, Wire, Rod

Titanium Grade 1

ASTM B348, ASTM F67, ISO 5832-2

Showing 1 to 10 of 16 entries

Previous

1
2

Next

Locations

Germany

Germany

Am Wall 127

28195 Bremen

(+49)421162270