ezcan A.Ş., which has a steel service production center along with the cold sheet, galvanized sheet, and painted sheet production processes in the same body, has cleaned hot sheet suitable for cold forming and deep drawing processes, suitable for cold forming, in line with the demands of the building, white goods and automotive sectors. manufactures galvanized steels and painted galvanized steels, non-alloyed structural steels, cold rolled sheets suitable for cold forming.
Headquarters
Kartepe,Kocaeli Province, Turkey
Website
Type
Manufacturer and Processor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
EN DC01 | Strip, Coil | EN DC01, EN 1.0330 | TS EN 10130 |
EN DC03 | Strip, Coil | EN DC03, EN 1.0347 | TS EN 10130 |
EN DC04 | Strip, Coil | EN DC04, EN 1.0338 | TS EN 10130 |
EN DX51D | Strip, Coil | EN DX51D, EN 1.0917 | TS EN 10346 |
EN DX52D | Strip, Coil | EN DX52D, EN 1.0918 | TS EN 10346 |
EN DX53D | Strip, Coil | EN DX53D, EN 1.0951 | TS EN 10346 |
EN DX54D | Strip, Coil | EN DX54D, EN 1.0952 | TS EN 10346 |
EN S220GD | Strip, Coil | EN S220GD, EN 1.0241 | TS EN 10346 |
EN S250GD | Strip, Coil | EN S250GD, EN 1.0242 | TS EN 10346 |
EN S280GD | Strip, Coil | EN S280GD, EN 1.0244 | TS EN 10346 |