General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Density of 1.55 g/cm³ | ASTM D792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Flexural modulus | 23.0 °C | 1.79 GPa Show Supplier Material materials with Flexural modulus of 1.79 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 75.8 MPa Show Supplier Material materials with Flexural strength of 75.8 MPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 530 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 530 J/m | ASTM D256 |
Tensile strength | 23.0 °C | 66.2 MPa Show Supplier Material materials with Tensile strength of 66.2 MPa | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 171 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 171 °C | ASTM D648 |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber |