Coefficient of friction, static: 0.5 [-]

Quick Comparison

Polyphenylene Sulfide (PPS)

LNP™ THERMOCOMP™ Compound OF008

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RF206

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DFL42

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DFL34EH

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFP36L

Geliefert von:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ THERMOCOMP™ Compound OF008H

Geliefert von:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL36 - Europe

Geliefert von:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL36R

Geliefert von: