Wrought Copper Nickel Silver Grade
EN 12164 Grade CuNi12Zn30Pb1 R420Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R590Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R540Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R640Other Copper Zinc Alloy
EN 12168 Grade CuZn37Mn3Al2PbSi H130Other Copper Zinc Alloy
EN 12168 Grade CuZn37Mn3Al2PbSi H150Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi H170Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R390Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R470Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R570Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R620Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R540Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn27 R600Wrought Copper Nickel Silver Grade
EN 12164 Grade CuNi12Zn30Pb1 R650Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn30Pb1 R430