Polyamide 66 (PA66)
Zytel® 70G33HS1L NC010Polyamide 66 (PA66)
Zytel® 70G33L NC010Polyamide 6T (PA6T)
Zytel® HTN51G45HSL NC010Polyethylenterephthalat (PET)
Rynite® 530 NC010Polyamide 66 (PA66)
Minlon® 11C40 NC010Polyamide 6 (PA6)
Zytel® 7335F NC010Polyoxymethylen (POM)
Delrin® 500CL NC010Polyphthalamid (PPA)
Zytel® HTN54G15HSLR NC010Polyethylenterephthalat (PET)
Rynite® 940 BK505Polyethylenterephthalat (PET)
Rynite® 530HTE NC010