Dehnung A5: 2.5 - 4.5 %

Quick Comparison

Cast Copper Bronze Aluminium Bronze

AMPCO® M4 Sand castings

Geliefert von:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

AMPCO® M4 Forged plates

Geliefert von:

AMPCO METAL

Wrought Copper High Copper Alloy

AMPCOLOY® 83 Extrusions

Geliefert von:

AMPCO METAL

Wrought Copper High Copper Alloy

AMPCOLOY® 944 Forgings

Geliefert von:

AMPCO METAL

Kohlenstoffarmer Stahl

JIS G3444 Grade STK500

Kohlenstoffarmer Stahl

JIS G3445 Grade STKM12C

Kohlenstoffarmer Stahl

JIS G3445 Grade STKM13B

Kohlenstoffarmer Stahl

JIS G3445 Grade STKM15C

Kohlenstoffarmer Stahl

JIS G3445 Grade STKM19C

Kohlenstoffarmer Stahl

JIS G3473 Grade STC440

Kohlenstoffarmer Stahl

JIS G3445 Grade STKM13C

Kohlenstoffarmer Stahl

JIS G3445 Grade STKM18C

Kohlenstoffarmer Stahl

JIS G3473 Grade STC510A

Kohlenstoffarmer Stahl

JIS G3473 Grade STC590A

Medium Carbon Steel

JIS G3445 Grade STKM17C

Medium Carbon Steel

JIS G3445 Grade STKM16A

Medium Carbon Steel

JIS G3445 Grade STKM16C

Medium Carbon Steel

JIS G3445 Grade STKM17A