Chromium Molybdenum Steel
EN 10132-3 Grade 25CrMo4 soft annealed or soft annealed and skin passed (+A or +A+LC)Medium Carbon Steel
EN 10132-3 Grade C40E soft annealed or soft annealed and skin passed (+A or +A+LC)Kohlenstoffarmer Stahl
ASTM A512 Grade 1016 Stress Relief Annealed Round TubesKohlenstoffarmer Stahl
ASTM A512 Grade 1018 Stress Relief Annealed Round TubesKohlenstoffarmer Stahl
ASTM A512 Grade 1110 Stress Relief Annealed Round TubesKohlenstoffarmer Stahl
ASTM A512 Grade 1115 Stress Relief Annealed Round TubesKohlenstoffarmer Stahl
ASTM A512 Grade MT1010 Stress Relief Annealed Round TubesKohlenstoffarmer Stahl
ASTM A512 Grade MT1015 Stress Relief Annealed Round TubesKohlenstoffarmer Stahl
JIS G3141 Grade SPCD 1/2 hardKohlenstoffarmer Stahl
JIS G3141 Grade SPCE 1/2 hardKohlenstoffarmer Stahl
JIS G3141 Grade SPCC 1/2 hardHartstahl
JIS G4802 Grade CS60 annealedKohlenstoffarmer Stahl
ASTM A109 Grade No. 1 HardMedium Carbon Steel
ASTM A513 Grade 1030 DOMKohlenstoffarmer Stahl
JIS G3539 Grade SWCH10KKohlenstoffarmer Stahl
JIS G3539 Grade SWCH12AKohlenstoffarmer Stahl
JIS G3539 Grade SWCH12KKohlenstoffarmer Stahl
JIS G3539 Grade SWCH12RKohlenstoffarmer Stahl
JIS G3539 Grade SWCH15A