Heat deflection temperature, 0.45 MPa: 174 °C

Quick Comparison

Polyoxymethylen (POM)

Delrin® 510GR NC000

Polyphenylether (PPE)

LNP™ THERMOCOMP™ Compound ZKC08

Geliefert von:

Sabic

Polyamide 11 (PA11)

LNP™ LUBRICOMP™ Compound HAL23

Geliefert von:

Sabic