Heat deflection temperature, 0.45 MPa: 293 °C

Quick Comparison

Polyphthalamid (PPA)

LNP™ LUBRICOMP™ Compound UFL36AS

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ THERMOCOMP™ Compound UF00BAS

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ THERMOCOMP™ Compound UF006H

Geliefert von:

Sabic