Impact strength, Izod notched, ASTM: 111 J/m

Quick Comparison

Polyphenylether (PPE)

NORYL™ Resin NH5120 - Europe

Geliefert von:

Sabic

Polyphenylether (PPE)

NORYL™ Resin NH5120 - Asia

Geliefert von:

Sabic