Description

LEXAN HP1 is a high flow polycarbonate (PC) with an MVR (300°C/1.2kg) of 25. This is a biocompatible (ISO10993 or USP Class VI) grade for medical devices and pharmaceutical applications. It is EtO and steam sterilizable, contains mold release and adheres to our healthcare management of change policy.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Material materials with Density of 1.19 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.15 %

Show Material materials with Water absorption of 0.15 %

ASTM D 570 | 24 Hours

Water absorption, equilibrium

100.0 °C

0.58 %

Show Material materials with Water absorption, equilibrium of 0.58 %

ASTM D 570 | ASTM D 570

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.37 GPa

Show Material materials with Elastic modulus of 2.37 GPa

ASTM D 638 | 50 mm/min

Elongation

23.0 °C

120 %

Show Material materials with Elongation of 120 %

ASTM D 638 | Type I, 50 mm/min

Elongation at yield

23.0 °C

6 %

Show Material materials with Elongation at yield of 6 %

ASTM D 638 | Type I, 50 mm/min

Flexural modulus

23.0 °C

2.3 GPa

Show Material materials with Flexural modulus of 2.3 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

90 MPa

Show Material materials with Flexural yield strength of 90 MPa

ISO 178 | 2 mm/min

Hardness, Rockwell M

23.0 °C

70 [-]

Show Material materials with Hardness, Rockwell M of 70 [-]

ASTM D 785

Hardness, Rockwell R

23.0 °C

118 [-]

Show Material materials with Hardness, Rockwell R of 118 [-]

ASTM D 785

Impact strength, Charpy notched

-30.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

23.0 °C

12 kJ/m²

Show Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

10 kJ/m²

Show Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A

23.0 °C

12 kJ/m²

Show Material materials with Impact strength, Izod notched of 12 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod notched, ASTM

23.0 °C

106.8 - 640.8 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 106.8 - 640.8 J/m

ASTM D 256

Impact strength, Izod unnotched, ASTM

23.0 °C

3204 J/m

Show Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m

ASTM D 4812

Tensile strength

23.0 °C

65 MPa

Show Material materials with Tensile strength of 65 MPa

ASTM D 638 | Type I, 50 mm/min

Yield strength

23.0 °C

62 MPa

Show Material materials with Yield strength of 62 MPa

ASTM D 638 | Type I, 50 mm/min

Impact strength, Izod unnotched

No Break @ 23,-30°C| ISO 180/1U

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6.84E-5 1/K

Show Material materials with Coefficient of thermal expansion of 6.84E-5 1/K

ASTM E 831 | -40°C to 95°C

Heat deflection temperature, 1.80 MPa

126 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 126 °C

ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B

Relative temperature index, mechanical impact

130 °C

Show Material materials with Relative temperature index, mechanical impact of 130 °C

UL 746B

Relative temperature index, mechanical strength

130 °C

Show Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B

Specific heat capacity

23.0 °C

1250 J/(kg·K)

Show Material materials with Specific heat capacity of 1250 J/(kg·K)

ASTM C 351

Thermal conductivity

23.0 °C

0.2 W/(m·K)

Show Material materials with Thermal conductivity of 0.2 W/(m·K)

ISO 8302

Vicat softening temperature

140 °C

Show Material materials with Vicat softening temperature of 140 °C

ISO 306 | Rate B/120

Flammability

UL Recognized, 94V-2 Flame Class Rating | 1.09mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

2 V

Show Material materials with Comparative tracking index of 2 V

UL 746A

Dielectric constant

23.0 °C

2.96 [-]

Show Material materials with Dielectric constant of 2.96 [-]

ASTM D 150 | at 1 MHz

Dielectric strength

23.0 °C

14.9 kV/mm

Show Material materials with Dielectric strength of 14.9 kV/mm

ASTM D 149 | in air, 3.2 mm

Dissipation factor

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor of 0.01 [-]

ASTM D 150 | at 1 MHz

Optical

PropertyValueComment

Haze

1 %

Show Material materials with Haze of 1 %

ASTM D 1003 | 2.54 mm

Refractive index

1.59 [-]

Show Material materials with Refractive index of 1.59 [-]

ASTM D542

Transmission

88 %

Show Material materials with Transmission of 88 %

ASTM D 1003 | 2.54 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

25 g/10min

Show Material materials with Melt mass-flow rate of 25 g/10min

ASTM D 1238 | 300°C/1.2 kg

Melt volume-flow rate

23 cm³/10min

Show Material materials with Melt volume-flow rate of 23 cm³/10min

ISO 1133 | 300°C/1.2 kg

Shrinkage

23.0 °C

0.5 - 0.7 %

Show Material materials with Shrinkage of 0.5 - 0.7 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Data Transfer,Displays,Enclosure/Housing/Cover,Enclosures,Fluid Delivery,Fused Deposition Modeling (FDM),Heavy Vehicles,Lab Ware and Clinical Diagnostics,LED Lighting,Medical Device,Medical Facility Infrastructure,Monitoring and Imaging,Pharmaceutical Manufacturing,Pharmaceutical Packaging & Drug Delivery,Renal and Blood Handling,Respiratory,Surgical Devices,Surgical Tray,Wireless Communications

Processing methods

Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 270-295°C, Nozzle Temperature: 265-290°C, Front - Zone 3 Temperature: 270-295°C, Middle - Zone 2 Temperature: 260-280°C, Rear - Zone 1 Temperature: 250-270°C, Mold Temperature: 70-95°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm