Impact strength, Izod notched, ASTM: 865 J/m

Quick Comparison

Polycarbonat (PC)

LEXAN™ Copolymer EXL1414 - Europe

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Copolymer EXL1444 - Americas

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Copolymer EXL1444 - Europe

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Copolymer FXE1414 - Americas

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Copolymer EXL1414H - Europe

Geliefert von:

Sabic