Impact strength, Izod notched, ASTM: 28 J/m

Quick Comparison

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IBP34

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KA000M

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

VALOX™ Resin 176

Polyethylen hoher Dichte (PE-HD)

SABIC® HDPE M300054