Polyphenylene Sulfide (PPS)

LNP™ THERMOCOMP™ Compound OF006

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ LUBRICOMP™ Compound WFL369

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DX11411R

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ STAT-KON™ Compound EE004

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DEL339XF

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DX05475

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DE0049P

Geliefert von:

Sabic

Acrylnitril-Butadien-Styrol (ABS)

LNP™ FARADEX™ Compound AS002

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DBL349E

Geliefert von:

Sabic

Acrylnitril-Styrol-Acrylat (ASA)

GELOY™ Resin CR7020

Acrylnitril-Styrol-Acrylat (ASA)

GELOY™ Resin CR7520

Polyetherimid (PEI)

LNP™ STAT-KON™ Compound EX01407C

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DX04489C

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound REL33

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ FARADEX™ Compound WX94736

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DE0029

Geliefert von:

Sabic

Polyamide 6 (PA6)

LNP™ THERMOCOMP™ Compound PF004S

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF006H

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF006XXZ

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ STAT-KON™ Compound KS000MXL

Geliefert von:

Sabic
Seite 1 von 3