Impact strength, Izod notched, ASTM: 73 J/m

Quick Comparison

Polymermischung (Blend)

XYLEX™ Resin X8300

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DE004

Geliefert von:

Sabic