XYLEX™ Resin X8300

Want to keep this datasheet? Save it now in your required format

Description

PC+Polyester, UV Stabilized, Transparent

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Material materials with Density of 1.2 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.2 %

Show Material materials with Water absorption of 0.2 %

ISO 62 | 23°C, 50% RH

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.52 GPa

Show Material materials with Elastic modulus of 1.52 GPa

ASTM D 638 | 50 mm/min

Elongation

23.0 °C

150 %

Show Material materials with Elongation of 150 %

ASTM D 638 | Type I, 50 mm/min

Elongation at yield

23.0 °C

5 %

Show Material materials with Elongation at yield of 5 %

ASTM D 638 | Type I, 50 mm/min

Flexural modulus

23.0 °C

1.7 GPa

Show Material materials with Flexural modulus of 1.7 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

78 MPa

Show Material materials with Flexural strength of 78 MPa

ISO 178

Flexural yield strength

23.0 °C

71 MPa

Show Material materials with Flexural yield strength of 71 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Hardness, Shore D

23.0 °C

73 [-]

Show Material materials with Hardness, Shore D of 73 [-]

ASTM D 2240

Impact strength, Charpy notched

23.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

7 kJ/m²

Show Material materials with Impact strength, Izod notched of 7 kJ/m²

ISO 180/1A

-10.0 °C

5 kJ/m²

Show Material materials with Impact strength, Izod notched of 5 kJ/m²

ISO 180/1A

23.0 °C

8 kJ/m²

Show Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

-30.0 °C

73 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 73 J/m

ASTM D 256

23.0 °C

1120 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 1120 J/m

ASTM D 256

Unlock all property charts

Tensile strength

23.0 °C

46 MPa

Show Material materials with Tensile strength of 46 MPa

ASTM D 638 | Type I, 50 mm/min

Yield strength

23.0 °C

47 MPa

Show Material materials with Yield strength of 47 MPa

ASTM D 638 | Type I, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.05E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-4 1/K

ASTM E 831 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

1.05E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.05E-4 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

75 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 75 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Thermal conductivity

23.0 °C

0.23 W/(m·K)

Show Material materials with Thermal conductivity of 0.23 W/(m·K)

ISO 8302

Vicat softening temperature

91 °C

Show Material materials with Vicat softening temperature of 91 °C

ASTM D 1525 | Rate B/50

Flammability

UL Recognized, 94V-2 Flame Class Rating | 3mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

0 V

Show Material materials with Comparative tracking index of 0 V

UL 746A

Optical

PropertyValueComment

Haze

1 %

Show Material materials with Haze of 1 %

ASTM D 1003 | 2.54 mm

Refractive index

1.54 [-]

Show Material materials with Refractive index of 1.54 [-]

ISO 489

Transmission

88 %

Show Material materials with Transmission of 88 %

ASTM D 1003 | 2.54 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

15 g/10min

Show Material materials with Melt mass-flow rate of 15 g/10min

ASTM D 1238 | 265°C/2.16kgf

Melt volume-flow rate

15 cm³/10min

Show Material materials with Melt volume-flow rate of 15 cm³/10min

ISO 1133 | 265°C/2.16 kg

Shrinkage

23.0 °C

0.5 - 0.8 %

Show Material materials with Shrinkage of 0.5 - 0.8 %

SABIC method | 3.2 mm

Shrinkage, transverse

23.0 °C

0.4 - 0.6 %

Show Material materials with Shrinkage, transverse of 0.4 - 0.6 %

SABIC method

Technological properties

Property
Application areas

Amusement Machine,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,EV Infrastructure,Lab Ware and Clinical Diagnostics,Laundry Dryer,LED Lighting,Medical Device,Medical Facility Infrastructure,Non-LED Lighting,Personal Care,Plumbing,Respiratory,Safety Glasses,Surgical Devices,Swimming Pool/Spa,Washing Machine

Processing methods

Drying Temperature: 65-75°C, Drying Time: 3-5hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 245-265°C, Nozzle Temperature: 245-265°C, Front - Zone 3 Temperature: 245-265°C, Middle - Zone 2 Temperature: 240-260°C, Rear - Zone 1 Temperature: 240-250°C, Mold Temperature: 45-60°C, Back Pressure: 0.2-0.5MPa, Screw Speed: 20-100rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.013-0.02mm