Impact strength, Izod unnotched, ASTM: 1030 J/m

Quick Comparison

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RE007

Geliefert von:

Sabic

Ethylene Tetrafluoroethylene Copolymer (ETFE)

LNP™ THERMOCOMP™ Compound 2X04505

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RE006 - Americas

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RE006 - Asia

Geliefert von:

Sabic