Impact strength, Izod unnotched, ASTM: 124 J/m

Quick Comparison

Styrol-Acrylnitril (SAN)

LNP™ LUBRICOMP™ Compound BX03658N

Geliefert von:

Sabic

Duroplast-Polymer-matrix-verbundwerkstoff

Phenolic BR60 - Sheet

Geliefert von:

Norplex-Micarta