Schlagzähigkeit, Izod ungekerbt: 64 kJ/m²

Quick Comparison

Thermoplastischer Co-Polyester (TCP)

Hytrel® G5544

Polybutylenterephthalat (PBT)

LNP™ THERMOTUF™ Compound WF009N

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RC006XXH

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RCL36 - Americas

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RCL36 - Europe

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ THERMOTUF™ Compound WF006I - Americas

Geliefert von:

Sabic

Thermoplastic Polyolefin (TPO)

MULTIFLEX™ TPO 7003 SW BLK 25092

Thermoplastic Polyolefin (TPO)

MULTIFLEX™ TPO 4203 SI1 BLK 26179