Instrumented Impact, at Peak: 7 J

Quick Comparison

Polybutylenterephthalat (PBT)

LNP™ THERMOCOMP™ Compound WX05456

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL33

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DDF029

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ STAT-KON™ Compound KEP33

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DF00A1P

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ THERMOCOMP™ Compound UF006H

Geliefert von:

Sabic

Polyphenylether (PPE)

LNP™ THERMOCOMP™ Compound ZFM62P

Geliefert von:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OX88533

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ LUBRICOMP™ Compound UFL36S - Americas

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ THERMOCOMP™ Compound UC008H

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RFZ349XC

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DFZ22P

Geliefert von:

Sabic