Instrumented Impact, Total Energy: 5 J

Quick Comparison

Polyphenylene Sulfide (PPS)

LNP™ KONDUIT™ Compound OX11315

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF002SXS

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DX11411R

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ STAT-KON™ Compound KS000MXL

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RBL36XXJ

Geliefert von:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QFL32

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ LUBRICOMP™ Compound LX00430

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RZL16

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KX06415

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ LUBRICOMP™ Compound LGL33

Geliefert von:

Sabic

Polyphenylether (PPE)

LNP™ LUBRICOMP™ Compound ZX02622

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFN14

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KAL22M

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFI12

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ THERMOCOMP™ Compound UF00BAS

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ THERMOCOMP™ Compound WFB62

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ LUBRICOMP™ Compound LL002

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ THERMOCOMP™ Compound KZ002

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KFI12

Geliefert von:

Sabic