General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.76 g/cm³ Show Supplier Material materials with Density of 1.76 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.78 [-] Show Supplier Material materials with Relative density of 1.78 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 18.4 GPa Show Supplier Material materials with Elastic modulus of 18.4 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 0.3 % Show Supplier Material materials with Elongation of 0.3 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 21.4 GPa Show Supplier Material materials with Flexural modulus of 21.4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 84 MPa Show Supplier Material materials with Flexural strength of 84 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 1 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 1 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 3 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 54 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 54 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 5 J Show Supplier Material materials with Instrumented Impact, Total Energy of 5 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature | 238 - 275 °C Show Supplier Material materials with Heat deflection temperature of 238 - 275 °C | ||||
Heat deflection temperature, 0.45 MPa | 275 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 275 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 238 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 238 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Specific heat capacity | 23.0 °C | 1.26E-3 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 1.26E-3 J/(kg·K) | ASTM C 351 | ||
Thermal conductivity | 23.0 °C | 15 W/(m·K) Show Supplier Material materials with Thermal conductivity of 15 W/(m·K) | ASTM E 1461-07 | ?25*0.4mm disc | ||
Thermal conductivity, through-plane | 23.0 °C | 3.5 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 3.5 W/(m·K) | ASTM E 1461-07 | 10*10*3mm sample | ||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101364448- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101069096- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 400 V Show Supplier Material materials with Comparative tracking index of 400 V | IEC 60112 | |
Dielectric strength | 23.0 °C | 1.2 kV/mm Show Supplier Material materials with Dielectric strength of 1.2 kV/mm | IEC 60243-1 | 1.6 mm |
Sheet resistivity, ROA | 23.0 °C | 2.40E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 2.40E+15 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Swimming Pool/Spa, Non-LED Lighting, LED Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |