Leaded Tin Bronze
ASTM B505 Grade C94300Leaded Tin Bronze
ASTM B505 Grade C94300Leaded Tin Bronze
ASTM B271 Grade C94300 As-CastLeaded Tin Bronze
ASTM B584 Grade C94300Leaded Tin Bronze
ASTM B763 Grade C94300 Separately Cast Test BarsLeaded Tin Bronze
ISO 4383 Grade CuPb24Sn4Copper-Lead Alloy
GOST 493 Grade BrS30Copper-Lead Alloy
ISO 4383 Grade CuPb30Copper-Lead Alloy
GB 1176 Grade CuPb30Gusskupfer
CEN/TS 13388 Grade 423184Gusskupfer
CEN/TS 13388 Grade 423187Gusskupfer
CEN/TS 13388 Grade 423188Kupfer
ASTM B66 Grade C94300