CEN/TS 13388 Grade 423187

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

27 - 33 %

Show Material materials with Lead of 27 - 33 %

Nickel

0.1 %

Show Material materials with Nickel of 0.1 %

Other

total 0.5

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silver

1.4 - 1.7 %

Show Material materials with Silver of 1.4 - 1.7 %

Tin

0.1 - 0.7 %

Show Material materials with Tin of 0.1 - 0.7 %

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %