Melt viscosity: 110 Pa·s

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2950-05

Geliefert von:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2900-04

Geliefert von:

Arkema: High Performance Polymers

Polybutylenterephthalat (PBT)

VALOX™ Resin 4012G

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 Black