Proportionalitätsgrenze bei der Kompression: 310 MPa

Quick Comparison

Cast Copper Bronze Aluminium Bronze

AMPCO® 18.23 Centrifugal castings

Geliefert von:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 18.23 Continuous cast

Geliefert von:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 18.23 Sand castings

Geliefert von:

AMPCO METAL