AMPCO® 18.23 Continuous cast

Want to keep this datasheet? Save it now in your required format

Description

This heat-treated alloy is the ultimate in high-strength bronzes requiring good bearing characteristics and exceptional wear resistance. It has greater toughness than grade AMPCO® 18.22 and better physical properties than grades AMPCO® 18 or AMPCO® 18.136. Its exceptional proportional limit gives it a maximum resistance to distortion, enabling the designer to take full advantage of its high physical properties.

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.45 g/cm³

Show Supplier Material materials with Density of 7.45 g/cm³

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

15 J

Show Supplier Material materials with Charpy impact energy of 15 J

Compressive strength

23.0 °C

1034 MPa

Show Supplier Material materials with Compressive strength of 1034 MPa

Elastic modulus

23.0 °C

110 GPa

Show Supplier Material materials with Elastic modulus of 110 GPa

Elongation A5

23.0 °C

15 %

Show Supplier Material materials with Elongation A5 of 15 %

Fatigue strength

23.0 °C

241 MPa

Show Supplier Material materials with Fatigue strength of 241 MPa

100.000.000 cycles

Hardness, HBW

23.0 °C

204 [-]

Show Supplier Material materials with Hardness, HBW of 204 [-]

HBW 10/3000

Hardness, Rockwell B

23.0 °C

94 [-]

Show Supplier Material materials with Hardness, Rockwell B of 94 [-]

Izod impact energy

23.0 °C

22 J

Show Supplier Material materials with Izod impact energy of 22 J

Proportional limit

23.0 °C

214 MPa

Show Supplier Material materials with Proportional limit of 214 MPa

Proportional limit in compression

23.0 °C

310 MPa

Show Supplier Material materials with Proportional limit in compression of 310 MPa

Reduction of area

23.0 °C

15 %

Show Supplier Material materials with Reduction of area of 15 %

Shear strength

23.0 °C

410 MPa

Show Supplier Material materials with Shear strength of 410 MPa

Tensile strength

23.0 °C

741 MPa

Show Supplier Material materials with Tensile strength of 741 MPa

Yield strength Rp0.5

23.0 °C

375 MPa

Show Supplier Material materials with Yield strength Rp0.5 of 375 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.62E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-5 1/K

Specific heat capacity

23.0 °C

420 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K)

Thermal conductivity

23.0 °C

59 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 59 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

7.50E+6 S/m

Show Supplier Material materials with Electrical conductivity of 7.50E+6 S/m

Specific Electrical conductivity

13 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 13 % IACS

Chemical properties

PropertyValue

Aluminium

10.5 %

Show Supplier Material materials with Aluminium of 10.5 %

Copper

Balance

Iron

3.5 %

Show Supplier Material materials with Iron of 3.5 %

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

Technological properties

Property
Application areas

AMPCO® 18.23 gives a successful performance under heavy loads and impact conditions and makes it a preferred material for heavy-duty worm gears and similar applications.