Zugfestigkeit, transversal: 2800 MPa

Quick Comparison

Cobalt Matrix Composite

S25T (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTE30A (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTS17R (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTE40M (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTE50A (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTM17E (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTM18-BC (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTS07M (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTF08M (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

KCR06+ (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

KCR10 (cemented carbide)

Geliefert von:

CERATIZIT