Red Brass
ASTM B505 Grade C83600Red Brass
ASTM B505 Grade C84200Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14500 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14510 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14520 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14700 H04Red Brass
ASTM B505 Grade C84200Wrought Copper Nickel Grade
ASTM B283 Grade C70620 M10Wrought Copper Nickel Grade
ASTM B466 Grade C71000 O60Wrought Copper Nickel Grade
ASTM B111 Grade C71000 O61Wrought Copper Nickel Grade
ASTM B111 Grade C72200 O61Leaded Brass
ASTM B16 Grade C36000 H02 (half-hard)Leaded Brass
ASTM B16 Grade C36000 O60 (soft anneal)Leaded Brass
ASTM B453 Grade C33500 H01Leaded Brass
ASTM B453 Grade C33500 H02Leaded Brass
ASTM B453 Grade C33500 O60Leaded Brass
ASTM B453 Grade C34000 H01Leaded Brass
ASTM B453 Grade C34000 H02Leaded Brass
ASTM B453 Grade C34000 O60Leaded Brass
ASTM B453 Grade C34500 H01