This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Elongation A50 A50
0 - 20 % at 20 °C
Hardness, Rockwell B HRB
0 - 80 [-] at 20 °C
Tensile strength Rm
0 - 395 MPa at 20 °C
Yield strength Rp0.5 Rp0.5
0 - 170 MPa at 20 °C
Element
Weight %
Comment
60 - 63 %
2.5 - 3 %
0 - 0.35 %
This material data has been provided by ASTM.