Streckgrenze Rp0,5: 195 MPa

Quick Comparison

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14500 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14510 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14520 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14700 H04

Cast Copper Bronze Aluminium Bronze

ASTM B148 Grade C95600 As-Cast

Other Copper Zinc Alloy

ASTM B371 Grade C69700 H04

Other Copper Zinc Alloy

ASTM B371 Grade C69710 H04

Cast Copper Bronze Aluminium Bronze

ASTM B763 Grade C95600 Separately Cast Test Bars

Wrought Copper High Copper Alloy

ASTM B301 Grade C18700 H04

Unclassified Carbon Steel

ASTM A663 Grade 345
Seite 1 von 2