Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 35 % Show Material materials with Elongation A50 of 35 % |
Tensile strength | 20.0 °C | 450 - 485 MPa Show Material materials with Tensile strength of 450 - 485 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 180 - 195 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 180 - 195 MPa |
Yield strength Rp0.5 | 20.0 °C | 195 - 205 MPa Show Material materials with Yield strength Rp0.5 of 195 - 205 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 6 - 8 % Show Material materials with Aluminium of 6 - 8 % |
Iron | 1.5 - 3.5 % Show Material materials with Iron of 1.5 - 3.5 % |
Lead | 0.01 % Show Material materials with Lead of 0.01 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |