Alpha-Beta-Legierung
AMS 4918 Grade R56620Alpha-Beta-Legierung
AMS 4918 Grade R56620Alpha-Beta-Legierung
AMS 4918 Grade R56620Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 34CrNiMo6 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10277-5 Grade 30CrMoV9 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10277-5 Grade 30CrNiMo8 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 cold drawn or turned and quenched and temperedChromium Molybdenum Steel
EN 10297-1 Grade 30CrMoV9 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10297-1 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10297-1 Grade 34CrNiMo6 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10263-4 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10263-4 Grade 34CrNiMo6 quenched and tempered (+QT)Betalegierung
DIN 17864 Grade TiAl6Zr5Mo0.5Si Artificially AgedAustenitischer rostfreier Stahl
SAE J775 Grade EV-17 For Mechanical Tests: ST+CWAustenitischer rostfreier Stahl
ASTM A666 Grade 205 Full HardAustenitischer rostfreier Stahl
ASTM A666 Grade 301 Full HardAustenitischer rostfreier Stahl
ASTM A666 Grade 302 Full Hard