Nickel Chromium Molybdenum Steel
EN 10263-3 Grade 21NiCrMo2 annealed to achieve spheroidized carbides (+AC)Nickel Chromium Molybdenum Steel
EN 10263-3 Grade 21NiCrMo2 annealed to achieve spheroidized carbides and turnedNickel Chromium Molybdenum Steel
EN 10263-3 Grade 21NiCrMo2 cold drawn, annealed to achieve spheroidized carbides and slightly skin passedNickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 treated to ferritic-pearlite structure and cold-drawnNickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 cold drawnNickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 cold-drawn or peeled and treated to ferrite-pearlite structureNickel Chromium Molybdenum Steel
DIN 1652-3 Grade 21NiCrMo2 cold drawn or turned and soft annealedNickel Chromium Molybdenum Steel
EN 10084 Grade 20NiCrMo2-2 quenched (+Q)Nickel Chromium Molybdenum Steel
DIN 17210 Grade 21NiCrMo2 soft annealed (+A)Nickel Chromium Molybdenum Steel
ASTM A752 Grade 8620 AnnealedNickel Chromium Molybdenum Steel
ASTM A837 Grade 8620Nickel Chromium Molybdenum Steel
JIS G4805 Grade 20NiCrMo2 annealed (soft annealed)Nickel Chromium Molybdenum Steel
JIS G4805 Grade 20NiCrMo2 annealed to achieve spheroidized carbidesNickel Chromium Molybdenum Steel
JIS G4805 Grade 20NiCrMo2 isothermally treated to ferrite-perlite structure and hardness rangeNickel Chromium Molybdenum Steel
JIS G4805 Grade 20NiCrMo2 treated to hardness rangeNickel Chromium Molybdenum Steel
JIS G4103 Grade SNCM220Nickel Chromium Molybdenum Steel
ASTM A506 Grade 8620Chromium Molybdenum Steel
SAE J404 Grade 8620Nickel Chromium Molybdenum Steel
ASTM A304 Grade 8617HNickel Chromium Molybdenum Steel
ASTM A304 Grade 8620H