Austenitischer rostfreier Stahl
Sandvik 3R60™Geliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
EN 10088-1 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17456 Grade X3CrNiMo17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10028-7 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10312 Grade X3CrNiMo17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X5CrNiMo17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X5CrNiMo17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
EN 10216-5 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10250-4 Grade X3CrNiMo17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X3CrNiMo17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
JIS G4303 Grade SUS316 solution treatedAustenitischer rostfreier Stahl
JIS G4304 Grade SUS316 solution treatedAustenitischer rostfreier Stahl
JIS G4305 Grade SUS316 solution treatedAustenitischer rostfreier Stahl
JIS G3459 Grade SUS316TPAustenitischer rostfreier Stahl
JIS G3467 Grade SUS316TFAustenitischer rostfreier Stahl
JIS G3463 Grade SUS316TBAustenitischer rostfreier Stahl
JIS G3446 Grade SUS316TKAAustenitischer rostfreier Stahl
JIS G4306 Grade SUS316 hot-rolled and solution annealed