Phosphorbronze
DIN 17662 Grade 2.1010Phosphorbronze
MSZ 710-1 Grade Bz 2Phosphorbronze
GOST 5017 Grade BrOF2-0,25Phosphorbronze
CEN/TS 13388 Grade C-7110Phosphorbronze
NP 3639 Grade CuSn2Phosphorbronze
UNI 2527-1 Grade CuSn2Phosphorbronze
CEN/TS 13388 Grade CuSn2Phosphorbronze
ASTM C50500