Austenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiMoTi17-12-2 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10272 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiMoTi17-12-2 quenched (+Q)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X6CrNiMoTi17-12-2 quenched (+Q)Austenitischer rostfreier Stahl
EN 10217-7 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10250-4 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10222-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X6CrNiMoTi17-12-2 cold drawn and quenchedAustenitischer rostfreier Stahl
DIN 1654-5 Grade X6CrNiMoTi17-12-2 quenched and turnedAustenitischer rostfreier Stahl
EN 10088-1 Grade X6CrNiMoTi17-12-2 strain-hardened (+C700)Austenitischer rostfreier Stahl
DIN 5512-3 Grade X6CrNiMoTi17-12-2 strain-hardened (+C700)Austenitischer rostfreier Stahl
JIS G4303 Grade SUS316 solution treatedAustenitischer rostfreier Stahl
JIS G4303 Grade SUS316Ti solution treatedAustenitischer rostfreier Stahl
DIN 1654-5 Grade X6CrNiMoTi17-12-2 cold drawn, quenched and slightly skin passedAustenitischer rostfreier Stahl
JIS G4304 Grade SUS316 solution treatedAustenitischer rostfreier Stahl
JIS G4304 Grade SUS316Ti solution treatedAustenitischer rostfreier Stahl
JIS G4305 Grade SUS316 solution treatedAustenitischer rostfreier Stahl
JIS G4305 Grade SUS316Ti solution treated