Austenitischer rostfreier Stahl
EN 10028-7 Grade X5NiCrAlTi31-20 recrystallization annealed (+RA)Austenitischer rostfreier Stahl
EN 10028-7 Grade X5NiCrAlTi31-20 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X5NiCrAlTi31-20 recrystallization annealed (+RA)Austenitischer rostfreier Stahl
DIN 17460 Grade X5NiCrAlTi31-20 solution annealed (+AT)Austenitischer rostfreier Stahl
JIS G4902 Grade NCF800H annealedAustenitischer rostfreier Stahl
JIS G4901 Grade NCF718 ageing treatment after solution treatmentAustenitischer rostfreier Stahl
JIS G4901 Grade NCF800H solution treatedAustenitischer rostfreier Stahl
JIS G4902 Grade NCF718 ageing treatment after solution treatmentAustenitischer rostfreier Stahl
JIS G4902 Grade NCF718 solution treated