EN 1.7323

Quick Comparison

Chromium Molybdenum Steel

DIN 1652-3 Grade 20MoCrS4 cold drawn

Chromium Molybdenum Steel

EN 10084 Grade 20MoCrS4 quenched (+Q)

Chromium Molybdenum Steel

ASTM A322 Grade G41210