Chromium Molybdenum Steel
EN 10222-2 Grade 13CrMo4-5 normalized and tempered (+NT)Chromium Molybdenum Steel
EN 10222-2 Grade 13CrMo4-5 quenched and tempered (+QT)Chromium Molybdenum Steel
DIN 17155 Grade 13CrMo4-4 quenched and tempered (+QT)Chromium Molybdenum Steel
ASTM A182 F12 Class 2 Annealed or Normalized and TemperedChromium Molybdenum Steel
ASTM A336 Grade F12 Annealed or Normalized and Tempered