Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn40 R340Wrought Copper Brass Yellow Brass
EN 12164 Grade CuZn40 R400Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn40 R400Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuSP R250Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuSP R300Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuTeP R250Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuTeP R300Leaded Brass
EN 12168 Grade CuZn39Pb2 R410Wrought Copper Brass Yellow Brass
EN 12168 Grade CuZn40 O60Leaded Brass
EN 1652 Grade CuZn39Pb2 R360Leaded Brass
EN 12166 Grade CuZn39Pb2 H02Leaded Brass
EN 12166 Grade CuZn39Pb2 H04Leaded Brass
EN 12166 Grade CuZn39Pb2 R500Leaded Brass
EN 12166 Grade CuZn39Pb2 H01Leaded Brass
EN 12166 Grade CuZn39Pb3 H02Leaded Brass
EN 12164 Grade CuZn36Pb3 R400Leaded Brass
EN 12164 Grade CuZn36Pb3 R480Leaded Brass
EN 12166 Grade CuZn39Pb3 H04Leaded Brass
EN 12168 Grade CuZn40Pb2 H02Leaded Brass
EN 12166 Grade CuZn40Pb2 H04