EN 1564

Quick Comparison

Ductile (Nodular) Cast Iron

EN 1564 Grade GJS-1000-5 austempered

Ductile (Nodular) Cast Iron

EN 1564 Grade GJS-1200-2 austempered

Ductile (Nodular) Cast Iron

EN 1564 Grade GJS-800-8 austempered

Ductile (Nodular) Cast Iron

EN 1564 Grade GJS-1400-1 cast condition