Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.1 g/cm³ Show Supplier Material materials with Dichte of 2.1 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 0.2 - 0.3 % Show Supplier Material materials with Andere of 0.2 - 0.3 % | Chloride, Iron, Aluminum, Silicon |
Bor | 40 - 41.9 % Show Supplier Material materials with Bor of 40 - 41.9 % | |
Kalzium | 0.2 - 2 % Show Supplier Material materials with Kalzium of 0.2 - 2 % | |
Sauerstoff | 0.3 - 3 % Show Supplier Material materials with Sauerstoff of 0.3 - 3 % | |
Stickstoff | 50 - 58.3 % Show Supplier Material materials with Stickstoff of 50 - 58.3 % |