Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 5.68 g/cm³ Show Supplier Material materials with Dichte of 5.68 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.1 - 0.4 % Show Supplier Material materials with Aluminium of 0.1 - 0.4 % | as Alumina |
Andere | 0.2 % Show Supplier Material materials with Andere of 0.2 % | Titania, Calcium Oxide, Iron Oxide, Sodium Oxide |
Silizium | 0.01 - 0.05 % Show Supplier Material materials with Silizium of 0.01 - 0.05 % | as Silica |
Yttrium | 4 - 5 % Show Supplier Material materials with Yttrium of 4 - 5 % | as Yttria |
Zirkonium | 90 - 95 % Show Supplier Material materials with Zirkonium of 90 - 95 % | as Zirconia |