Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | |
Partikelgrößenbereich | 0.76 µm Show Supplier Material materials with Partikelgrößenbereich of 0.76 µm | ||
Partikelgröße | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 24.03 MPa Show Supplier Material materials with Biegefestigkeit of 24.03 MPa |
Biegefestigkeit, transversal | 23.0 °C | 20.01 MPa Show Supplier Material materials with Biegefestigkeit, transversal of 20.01 MPa |
Druckfestigkeit | 23.0 °C | 55.02 MPa Show Supplier Material materials with Druckfestigkeit of 55.02 MPa |
Druckfestigkeit, transversal | 23.0 °C | 55.02 MPa Show Supplier Material materials with Druckfestigkeit, transversal of 55.02 MPa |
Elastizitätsmodul | 23.0 °C | 10.96 GPa Show Supplier Material materials with Elastizitätsmodul of 10.96 GPa |
Elastizitätsmodul, transversal | 23.0 °C | 8.27 GPa Show Supplier Material materials with Elastizitätsmodul, transversal of 8.27 GPa |
Hardness, Rockwell R | 23.0 °C | 93 [-] Show Supplier Material materials with Hardness, Rockwell R of 93 [-] |
Zugfestigkeit | 23.0 °C | 19.02 MPa Show Supplier Material materials with Zugfestigkeit of 19.02 MPa |
Zugfestigkeit, transversal | 23.0 °C | 15 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 15 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.12 % Show Supplier Material materials with Aschegehalt of 0.12 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 23.0 °C | 170 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 170 W/(m·K) | |
Thermal conductivity, through-plane | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 130 W/(m·K) | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3.6E-6 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3.6E-6 1/K | average for 20-100°C |
Elektrisch
Technological properties
Property | ||
---|---|---|
Application areas | Casting molds and furnace parts for hot metal, Powder metallurgy, Boats and trays for sintering applications, Resistance heating, Crucibles for melting and alloying, Quartz processing | |
Processing history | Extruded |